Common stainless casting defects are porosity, shrinkage cavities, inclusions and hot tears. They are found by visual checks, dye penetrant, radiography or ultrasonic testing.
Defects
- Porosity: small gas holes
- Shrinkage cavities: voids where metal shrank as it cooled
- Inclusions: slag or sand trapped in the metal
- Hot tears: cracks formed while cooling
How they are found
Surface defects show up with dye penetrant testing. Internal defects need radiography (X-ray) or ultrasonic testing. Pressure parts are also hydro tested.
Related guides
- How to order power plant spares: What to include when requesting power plant spares: OEM, model, part numbers, drawings, nameplate photos and quantity, for a…
- OEM vs drawing-based spares: The difference between OEM spares and spares made to your drawing, with a checklist of what to verify before choosing either…
- What is stainless steel casting?: Stainless steel casting pours molten stainless steel into a mould to form complex shapes such as pump casings and valve…
- Stainless casting grades CF8 and CF8M: CF8, CF8M, CF3 and CF3M are common stainless steel casting grades under ASTM A351 and A743. See how they match wrought grades…
What to send us
- Spares list with part numbers
- Drawings and material specification
- OEM and equipment
- Delivery timeline and documents
About power plant spares from Asaus Technologies
Asaus Technologies is an independent supplier based in Vadodara, Gujarat, and supplies power plant spares across India. Spares and replacement components, matched to your drawings and part numbers. See the power plant spares page.
Need power plant spares?
Tell us the tests your specification requires. Request a quote.